CONCENTRATION AND TEMPERATURE DEPENDENCE ON THE PARTIAL SPECIFIC VOLUME OF POLYSTYRENE IN TETRALIN | ||||
International Conference on Aerospace Sciences and Aviation Technology | ||||
Article 67, Volume 1, A.S.A.T. CONFERENCE 14-16 May 1985 r CAIRO, May 1985, Page 797-806 PDF (1.22 MB) | ||||
Document Type: Original Article | ||||
DOI: 10.21608/asat.1985.26558 | ||||
![]() | ||||
Authors | ||||
ABDEL-AZIM A. ABDEL-AZIM1; M. B. HUGLIN2 | ||||
1Department of Chemistry, Military Technical College, Kobry El-Kobba, Cair, Egypt. | ||||
2Department of Chem. and Applied Chem., University of Salford, Salford M5 4WT, U.K. | ||||
Abstract | ||||
In the previous communications we have used the value of the partial specific volume, v2, of polystyrene, PS, derived by Hooker et al (1) for determining the molecular weight of the polymer by light scattering (2), viscosity slope constant (3,4) and the excluded volume parameter (5,6). The partial specific volume is a characteristic parameter of the polymer. This parameter depends on both intra- and inter molecular segment-segment interactions. Hence, several reports (7-11) considered the dependence of v2 on the solvent, concentration and temperature. Hence, specific volume measurements on solutions of PS sample in tetralin, Tet., at different temperatures and mass fractions were performed. | ||||