Effect of Different Veneering Techniques on Shear Bond Strength and Translucency of Bi-layered Zirconia Ceramics | ||||
Al-Azhar Dental Journal for Girls | ||||
Article 18, Volume 5, Supplement, October 2018, Page 557-565 PDF (283.65 K) | ||||
Document Type: Original Article | ||||
DOI: 10.21608/adjg.2018.109420 | ||||
View on SCiNiTO | ||||
Authors | ||||
Yousra Ibrahim* 1; Mona H. Mandour2; Rania A. Shetawey2 | ||||
1Demonstrator, Crowns and Bridges Department, Faculty of Dental Medicine, Al-Azhar University (Girls’ branch) | ||||
2Associate Professor, Crowns and Bridges Department, Faculty of Dental Medicine, Al-Azhar University (Girls’ branch). | ||||
Abstract | ||||
Purpose. This study was designed to compare the effect of different veneering techniques (CAD-on, Press-on and manual layering) on the shear bond strength of veneering ceramics to zirconia framework and translucency of bi-layered zirconia based ceramics. Materials and Methods: A total of forty-eight zirconia samples were fabricated and were divided into three equal groups (n=16) according to the veneering technique used: Group (I): samples veneered using CAD-on technique. Group (II): samples veneered using Press-on technique and Group (III): samples veneered using manual layering technique. The samples of each group were subdivided into two equal subgroups (n=8) according to the testing procedure: Subgroup (A): for translucency parameter (TP). Subgroup (B): for shear bond strength. All samples were thermocycled in thermocycling device. Samples of subgroup (A) were tested for translucency parameter (TP) by using a reflective spectrophotometer. Samples of subgroup (B) were tested by using a universal testing machine. Failure modes of fractured samples were evaluated using stereomicroscope and scanning electron microscope (SEM).Data were statistically analyzed. Results: CAD-on veneered samples, group (1), recorded higher mean translucency parameter (11.099±0.452) than manual layering veneered samples, group (3), which recorded lower translucency parameter (5.463±1.255). CAD-on veneered samples, group (1), recorded higher mean shear bond strength (16.262±4.492) than Press-on veneered samples, group (2) which recorded lower shear bond strength (8.584±1.606). Conclusions: CAD-on veneered samples showed superior translucency parameter and shear bond strength than Press-on veneered samples. | ||||
Keywords | ||||
Zirconia core; Shear bond strength; Translucency parameter; Digital veneering method | ||||