Debonding of lithium Disilicate and Felspathic Veneers with Er, Cr: YSGG laser bonded with two different curing mode resin cement. | ||||
Al-Azhar Journal of Dental Science | ||||
Article 3, Volume 24, Issue 1, January 2021, Page 19-26 PDF (1.11 MB) | ||||
Document Type: Original Article | ||||
DOI: 10.21608/ajdsm.2020.48964.1134 | ||||
View on SCiNiTO | ||||
Authors | ||||
Ghada Abdelfattahh Hussein 1; Norbert Gutknecht2; talaat samhan3; Ahmed Ibrahim Youssef4 | ||||
1Department of Fixed Prosthodontics, Faculty of Dentistry, Ain Shams University Organization of African Unity Street, Cairo, Egypt | ||||
2Dep. Director of the Department of Restorative Dentistry, Director of the Aachen Dental Laser Center, Scientific Director of Academic Postgraduate Master Program "Master of Science – Laser in Dentistry at the RWTH Aachen University | ||||
3Lecturer of Fixed Prosthodontics, Fixed prosthodontics Department, Faculty of Dentistry, Misr International University | ||||
4Assistant lecturer, Restorative department, Misr International University | ||||
Abstract | ||||
The purpose The purpose of this study was to evaluate the debonding of feldspathic and lithium disilicate reinforced glass ceramic veneers using Erbium lasers with two different curing mode resin cement.] Materials and Methods: In this study, a total of 80 ceramic specimens were used. They were divided into two groups (n= 40/group) according to ceramic material used into: Group (A) lithium disilicate (IPS Emax), Group (B) Feldspathic porcelain. (VITA MARK II). Each group was further subdivided into two subgroups according to the cement curing mode (n= 20/subgroup): Subgroup (L) Light cured resin cement, Subgroup (D) Dual cured resin cement. Er,Cr:YSGG (turbo handpiece) was used on all subgroups. Scanning electron microscope and Profilometer were used to evaluate surface tomography & roughness. Data was analyzed statistically. Results: For surface roughness of two ceramics at base line and after debonding .There was no statistically significant difference between median (Ra) values of the two ceramics (P-value=0.754, Effect size=0.199), (P-value= 0.825, Effect size=0.155) and (P-value=0.117, Effect size=0.245). As for the curing mode: both materials showed no statistically significant effect of curing modes (P-value = 0.425, Effect size = 0.051) and (P-value = 0.543, Effect size = 0.065), respectively. Conclusion: Based on the limitation of the current study ; the following conclusions can be drawn: -Er, Cr: YSGG fluid dynamic laser system is an effective clinical application for the debonding of resin-bonded all-ceramic restorations. - the surface topography of both ceramic materials almost the same after debonding which make their future use possible | ||||
Keywords | ||||
laser debonding; ceramic veneers; different curing modes | ||||