Comparison of Cyclic Fatigue Resistance of Two Different Rotary NiTi Instruments (An In-Vitro Study) | ||||
Ain Shams Dental Journal | ||||
Volume 33, Issue 1, March 2024, Page 121-126 PDF (1.22 MB) | ||||
Document Type: Original articles | ||||
DOI: 10.21608/asdj.2023.216874.1180 | ||||
View on SCiNiTO | ||||
Authors | ||||
Dalia Abd elmoez Abd allah 1; mohamed Nagy2; Tariq Yehia 3 | ||||
1Endodontics Department , ASU | ||||
2Endodontics Department, Faculty of Dentistry, Ain shams University | ||||
3EndodonticS Department, Faculty of Dentistry, Ain Shams University, Cairo, Egypt. | ||||
Abstract | ||||
Aim: The aim of this study was to compare the dynamic cyclic fatigue resistance of M3-ProGold files and Pepsi Gold Files. Materials and methods: Eighty files of size 25/.06 of M3 Pro Gold files and Pepsi Gold files (each n = 40) were evaluated for dynamic cyclic fatigue resistance inside two artificial stainless steel canals with 2 different radii [(60 curvature, 3 mm radius) and (60 curvature, 5 mm radius)] at body temperature while submerged in distilled water at 37 ° ± 1 °C. The NCF (number of cycles to failure) was calculated. The data of NCF were analyzed using ANOVA and Tukey post hoc tests (P ≤ 0 .05). Results: The Pepsi Gold files had a significantly higher number of cycles to failure than the M3 Pro Gold files in both canal radii at body temperature. Conclusion: Pepsi Gold files have greater resistance to cyclic fatigue than M3 Pro Gold files. | ||||
Keywords | ||||
Cyclic Fatigue; CM-Alloy; M3 Pro Gold files; Pepsi Gold files | ||||